Scintillation Coatings on Imaging and Line Sensors
發布時間: 2020-07-31 09:38
ProxiVision
Generally speaking phosphor coatings are used for the visualisation of energetic photons, Soft X-ray imaging, synchrotron radiation. The phosphor coating is prepared by sedimentation of phosphor grains on a solid state sensor like CCD or CMOS Sensor. Since these sensors are usually not sensitive for a wavelength < 350nm the coating acts as a spectral converter in most cases to green light. Coated solid state sensors are a much less expensive alternative to back thinned sensors if the other advantages of these sensors are not necessary for the application. Scintillation Coatings on Imaging and Line Sensors主要參數:
P43, P46, P47, P11 and other scintillators
segmentation of the coating area possible
Sensor sizes 100x100mm²
coating of line and area CCD/CMOS elements without protection window (Removing of the window is provided as a service)
coating thickness up to 25µm
Scintillation Coatings on Imaging and Line Sensors 特點: Our sedimentation process leads to a very homogeneous layer structure. To guarantee a homogeneous layer structure, at least 3 to 4 layers of phosphor grains are necessary. The minimum average grain size available is 1 µm. The maximum thickness of the phosphor coating is up to ca. 25µm.
The resolution limit RL is defined as the spatial frequency resulting in a modulation transfer function MTF with a value of 3%. RL is measured in linepairs/mm (lp/mm) and can be approximated as RL = 500/D (D as the thickness of the phosphor layer in µm). Up to 80lp/mm are possible. Scintillation Coatings on Imaging and Line Sensors 應用: